Origin |
China |
Ni/Diatomite (diatomaceous earth) composite powders consist of a diatomite core coated with a thin layer of nickel. It has the superior oxidation resistance, anti scour and thermal shock resistance.
The coatings obtained by thermo-spraying are oxidation resistant and heat-shock resistant at 750??nbsp;or below and air abradable seal applications. The coatings with oxidation resistant, anti scour and thermal shock resistance is combined the heat-resistant quality of the natural diatomaceous earth and the strength and good adhesion of Ni. It is used in the abradable seal coating at 750??nbsp;or below. Not only control the radial clearance of the turbine but also keep the sealing of the gas circuit of the gas compressor.
Specifications & compositions:**
|
No.
|
Chemical composition(wt%)
|
|
Ni
|
D.E
|
Major impurities
|
|
Al2O3
|
Fe
|
MgO
|
CaO
|
Na
|
|
CM04-1
|
75±1.5
|
The rest
|
<4.0
|
<1.0
|
<0.5
|
<0.2
|
<0.2
|
|
CM04-2
|
75±1.5
|
The rest
|
<4.0
|
<1.0
|
<0.5
|
<0.2
|
<0.2
|
|
CM04-3
|
75±1.5
|
The rest
|
<1.2
|
<2.0
|
<.12
|
-
|
<0.45
|
|
No.
|
Particle size range
(mesh)(wt%)
|
Apparent density
(g/cm3)
|
Flowability(s/50g)
|
|
+100
|
-200
|
-320
|
|
CM04-1
|
-
|
<40
|
<5
|
≥1.20
|
<95
|
|
CM04-2
|
-
|
<60
|
<10
|
>1.00
|
<110
|
|
CM04-3
|
-
|
<45
|
<10
|
≥0.95
|
<120
|
**Can be varied to meet the customers' requirement.
|